Flame Retardant TPV relatively more difficult coloring , usually our only should the white and black two kinds , if you need other colors , you need to customize ! But there is a direct customer's own color , it can speed up the progress of the color , but pay attention to the following questions : a) do not directly use toner , unless the customer's oil expeller; b) Optional masterbatch to PE or PP as the base material , and requires very good flowability and lubricity , c) the amount of added masterbatch generally in the 3-5 % .Because tough TPV Port TM retardant containing about 30% of the flame retardant , so the process is different conventional TPV , the following aspects are to be noted : Ren Hong Kong TM Flame Retardant TPV drying before oil refinery
To be dried before processing , dry conditions of 100 ° C / 2 hours, dried test is in place , you can view products and articles section apparent , if the apparent roughness and porosity found in a cross section , then need to be further dried.

没有评论:

发表评论