1, the boot, first warming of about forty to fifty minutes. The temperature rose to Pellet mill the motor by hand until the belt freely; continuous rotation at work pulling
Eight to ten times. Then continue to heat up about ten minutes, and then boot, but continue heating, because the normal production requires continuous supplement the heat;
Depending on the nature of the plastic regulate different temperatures.
2, granulating machine work, the machine temperature to maintain stability, not fluctuated. Bleed hole near the nose area Briquette machinee should be maintained until about 200 ℃
(Refers to the C material, material B).
3, the feed should be uniform, and add enough. Loom eat feed speed and feed rate to tie properly. Otherwise it will affect grain quality and yield.
4, shut down the host to completely cut off the power. Nose plugs (with wrench part) must come off. Subject to a separate warm-up before the next use.